Adhesion testing results on mini-module coupons (cell/encapsulant/glass laminates) that were aged under the following conditions.
- Hot-dry (90 Celsius, ~1% RH, no UV) for up to 10k hours
- Hot-humid (90 Celsius, ~60% RH, no UV) for up to 10k hours
- Warm-humid (60 Celsius, ~60% RH, no UV) for up to 10k hours
- IEC A3 (65 Celsius chamber setpoint, open-air, with UV source) for up to 10k hours
- IEC A3 for 2500 hours followed by Warm-humid for 2500 hours (1x sequence for 5k hours total, 2x sequence for 10k hours total)
- Warm-humid for 2500 hours followed by IEC A3 for 2500 hours (1x sequence for 5k hours total, 2x sequence for 10k hours total)
- IEC A3 for 2500 hours followed by warm-humid for 2500 hours followed by hot-dry for 2500 hours
Dataset Metadata
作成者 |
aliu1997
|
メンテナーのemail |
aliu1997@stanford.edu
|
Data Source Type |
Lab and Experimental
|
Accelerated? |
Yes
|
Environmental Conditions |
Steady State
|
Owner |
aliu1997
|
作成者 |
aliu1997
|
Updated |
9月 30, 2025, 16:02 (UTC)
|
作成日 |
9月 25, 2025, 21:58 (UTC)
|