Adhesion testing results on mini-module coupons (cell/encapsulant/glass laminates) that were aged under the following conditions.

  • Hot-dry (90 Celsius, ~1% RH, no UV) for up to 10k hours
  • Hot-humid (90 Celsius, ~60% RH, no UV) for up to 10k hours
  • Warm-humid (60 Celsius, ~60% RH, no UV) for up to 10k hours
  • IEC A3 (65 Celsius chamber setpoint, open-air, with UV source) for up to 10k hours
  • IEC A3 for 2500 hours followed by Warm-humid for 2500 hours (1x sequence for 5k hours total, 2x sequence for 10k hours total)
  • Warm-humid for 2500 hours followed by IEC A3 for 2500 hours (1x sequence for 5k hours total, 2x sequence for 10k hours total)
  • IEC A3 for 2500 hours followed by warm-humid for 2500 hours followed by hot-dry for 2500 hours

Dataset Metadata

Autor aliu1997
Email do Gestor aliu1997@stanford.edu
Data Source Type Lab and Experimental
Accelerated? Yes
Environmental Conditions Steady State
Owner aliu1997

Autor aliu1997
Updated Setembro 30, 2025, 16:02 (UTC)
Data de criação Setembro 25, 2025, 21:58 (UTC)